Abstract: 采用A型脉冲反射式超声检测壁厚大于4mm、外径为32mm~159mm的压力管道环向对接焊接接头,缺陷容易漏检。分析了漏检原因,提出了避免缺陷漏检的措施。
- DOI:
10.13689/j.cnki.cn21-1230/th.2015.03.016
- Series:
(C) Architecture/ Energy/ Traffic/ Electromechanics, etc
- Subject:
Instrument and Meter Industry
- Classification Code:
TH878
- Mobile Reading
Read on your phone instantly
Step 1
Scan QR Codes
"Mobile CNKI-CNKI Express" App
Step 2
Open“CNKI Express”
and click the scan icon in the upper left corner of the homepage.
Step 3
Scan QR Codes
Read this article on your phone.
- Download
- Online Reading
- AI Summary

Download the mobile appuse the app to scan this coderead the article.
Tips: Please download CAJViewer to view CAJ format full text.
Download: 125 Page: 44-46 Pagecount: 3 Size: 150K
Citation Network
Related Literature
- Similar Article
- Reader Recommendation
- Associated Author
- [1]小径管射线探伤缺陷精确定位的方法[J]. 唐欣. 青海科技. 2005(03)
- [2]考虑厚度宽容度的曝光曲线在小径管射线检测中的应用[J]. 李隆骏,王飞. 无损检测. 2007(12)
- [3]电站大修中小径管探伤存在的问题及其解决方法[J]. 吕胜军. 无损探伤. 1994(02)
- [4]小径管对接接头射线检测不同标准的参数选取探讨[J]. 刘洪会,马君鹏. 无损探伤. 2009(02)
- [5]小径管周向裂纹涡流传感器几何参数优化[J]. 王金凯,付跃文,王鑫,后雪冰. 无损检测. 2018(12)
- [6]厚壁小径管X射线透照新工艺应用[J]. 张东升,申景泉,李亚伟. 无损探伤. 1998(05)
- [7]小径管透照射线机位置指示器[J]. 何志春. 无损检测. 1999(06)
- [8]小径管超声波探伤缺陷漏检或误判原因浅析[J]. 莫学愚. 河北电力技术. 1996(05)
- [9]特殊位置小径管的射线探伤[J]. 叶永魁. 无损检测. 2006(04)
- [10]厚壁小径管X射线探伤实践[J]. 吴剑. 广西电力技术. 2000(01)