Investigation of mode Ⅰ-Ⅱ-Ⅲ fracture of brittle spheres with a 60° internal crack using 3D-ILCChinese Full Text
WANG Hai-jun;YU Shu-yang;TANG Zi-xuan;TANG Lei;REN Ran;XU Jin;State Key Laboratory of Hydrology-Water Resource and Hydraulic Engineering, Nanjing Hydraulic Research Institute;Collaborative Innovation Center on Water Safety and Water Science, Hohai University;Huatian Corporation, China Metallurgical Group Corporation;Ecole Nationale Supérieure de Techniques Industrielles et des Mines de Douai;
Abstract: As one of the perfect geometries in nature,sphere is common in the daily and industrial life.The mechanical properties of sphere are of great significance to engineering safety and numerical simulation.Internal cracks or defects are inherent properties of materials,and have an important influence on the mechanical properties of materials.However,the internal crack of sphere is not considered in the current research due to the limit of technology.Thus,understanding of the propagation of internal ... More
- DOI:
10.16285/j.rsm.2019.1071
- Series:
(C) Architecture/ Energy/ Traffic/ Electromechanics, etc; (A) Mathematics/ Physics/ Mechanics/ Astronomy
- Subject:
Geology; Architecture and Engineering
- Classification Code:
TU45
- Mobile Reading
Read on your phone instantly
Step 1
Scan QR Codes
"Mobile CNKI-CNKI Express" App
Step 2
Open“CNKI Express”
and click the scan icon in the upper left corner of the homepage.
Step 3
Scan QR Codes
Read this article on your phone.
- Download
- Online Reading
- AI Summary

Download the mobile appuse the app to scan this coderead the article.
Tips: Please download CAJViewer to view CAJ format full text.
Download: 226 Page: 1573-1582 Pagecount: 10 Size: 1676K
Citation Network
Related Literature
- Similar Article
- Reader Recommendation
- Associated Author
- [1]古断裂研究的几个问题[J]. 王丹. 西北地质. 1982(02)
- [2]断裂构造的有序性及断裂研究的三个阶段[J]. 孙文鹏,方茂龙,蔡文伯,徐道一. 地质论评. 2000(S1)
- [3]基于3D-ILC含水平内裂纹脆性固体三点弯断裂特性研究[J]. 王海军,乐成军,汤雷,赵初,李汉章,戚海棠. 岩土力学. 2021(10)
- [4]基于3D-ILC单轴拉伸双平行内裂纹扩展规律研究[J]. 郁舒阳,王海军,任然,汤雷,钟凌伟,张志韬,汤子璇. 岩土工程学报. 2019(12)
- [5]基于激光–介质损伤的三维内裂纹3D-ILC实现[J]. 王海军,张九丹,任然,汤雷,钟凌伟. 岩土工程学报. 2019(12)
- [6]基于3D-ILC含内裂纹孔口脆性固体断裂特性试验[J]. 王海军,郁舒阳,任然,汤雷,李欣昀,贾宇. 岩土力学. 2019(06)
- [7]带遗忘因子的ILC在桥式起重机防摆中的应用研究[J]. 贾胜,贺风华,刘海波,冯敏. 煤矿机械. 2017(09)
- [8]基于3D-ILC三点弯脆性固体内裂纹扩展规律及破坏特征研究[J]. 王海军,李汉章,任然,汤雷,郁舒阳,张志韬. 岩石力学与工程学报. 2019(12)
- [9]基于3D-ILC含60°平行双内裂纹脆性巴西圆盘断裂特性[J]. 王海军,张珂,任然,汤雷,郁舒阳. 工程科学与技术. 2020(04)
- [10]矿用重型汽车车架断裂研究[J]. 于长吉,王平一. 大连工学院学报. 1984(01)